4330V MOD chemical composition:
C
Mn
P
S
Si
Ni
Cr
Mo
V
0.28~0.37
0.45~0.65
≤0.015
≤0.015
0.1~0.3
2.0~3.0
0.80~1.10
0.4~0.65
0.05~0.15
Mechanical properties:
Tensile strength ≥1033Mpa(T) ≥1033Mpa(L)
Yield strength ≥964Mpa(T) ≥964Mpa(L)
Elongation rate ≥10.7%(T) ≥15%(L)
Impact energy ≥90J(T) ≥50J(L)
Face shrinking ≥32%(T) ≥45%(L)
Hardness 320-360HB